Graphite Crucible Liner For Induction Melting

A graphite crucible liner is the inner shell that sits inside a clay-graphite or silicon carbide crucible, or inside a water-cooled induction coil former. It is the part that actually contains the melt, and it is replaced on its own when the outer shell is still sound, which keeps the melting cost per tonne low.
Jincheng turns these liners from isostatic graphite with a wall thickness that balances thermal conduction against mechanical strength. The liner is machined with a matched taper to the outer crucible, a flat bottom, and a lip that sits above the melt line, so the metal does not bridge between the liner and the outer shell.
Key Features
-
Non-wetting inner surface - Metal does not stick to the liner, so the crucible cleans out between alloys and cross-contamination between melts is reduced.
-
Replaceable inner shell - When the liner wears through, only the liner is replaced; the outer crucible and the coil former stay in service.
-
Taper matched to the outer crucible - The outside profile is machined to the same taper as the host crucible, so the liner seats fully and heat transfers through the wall without an air gap.
-
Controlled wall thickness - Wall thickness is chosen so the liner heats through quickly but keeps enough strength to resist charging impact.
-
Lip above the melt line - A machined lip sits above the maximum melt level, which stops metal from bridging into the gap between liner and shell.
-
High-density, low-porosity grade - Dense isostatic graphite resists metal penetration, which is the main cause of liner failure in induction melting.
Technical Specifications
| Property | Typical Value |
| Material | Isostatic fine-grain graphite |
| Bulk density | 1.85 to 1.92 g/cm3 |
| Ash content | Below 0.1 percent |
| Open porosity | Below 10 percent |
| Top inside diameter | 100 to 500 mm |
| Bottom inside diameter | 80 to 450 mm |
| Liner height | 150 to 800 mm |
| Wall thickness | 10 to 40 mm |
| Bottom thickness | 15 to 50 mm |
| Taper | 1 to 5 degrees per side |
| Service temperature | Up to 2000 C in vacuum or inert gas |
| Typical life | 3 to 12 months depending on alloy and cycle count |
Applications & How to Use
Copper and bronze induction melting
The liner sits in a clay-graphite crucible; the charge is loaded against the liner wall and the melt is poured through a lip.
Precious metal melting
Dense liners prevent metal penetration, which matters when the melt value is high and contamination is expensive.
Aluminium alloy melting
A liner inside a silicon carbide crucible keeps iron pickup low compared with a bare clay-graphite shell.
Vacuum induction melting
Liners are used inside a water-cooled copper crucible in small VIM furnaces where the melt is contained by the graphite shell.
Alloy changeover
Where one furnace melts several alloys, a spare liner is swapped in so cross-contamination between campaigns is avoided.
Why Choose Jincheng
- The outside taper is machined to the host crucible, so the liner does not sit on a partial contact that overheats the wall.
- Dense, low-porosity graphite resists metal penetration, which is the usual cause of liner failure.
- A lip above the melt line stops metal bridging into the gap between liner and shell.
- Liners are supplied to the customer's melt volume, not to a catalogue size, so the metal depth is predictable.
- We keep the taper record so a replacement liner fits the same host crucible years later.
- Liners are packed in a crate with the bore supported and the lip protected.
FAQ
Why use a liner instead of a solid graphite crucible?
A liner lets a foundry keep the outer crucible and coil former in service and replace only the part that touches the melt, which lowers cost per melt.
How do I know the liner has worn out?
Watch for metal penetration on the outside wall, a change in melt time, or a bulge in the shell. A liner that has worn thin heats faster and then fails suddenly.
Can the liner be used in a clay-graphite crucible?
Yes, provided the taper matches. The liner is seated in the host crucible and the charge is loaded inside the liner.
Does the liner need preheating?
Yes. A slow preheat to 200 to 300 C removes moisture before the charge is added, which prevents a steam-driven crack.
What wall thickness do you recommend?
For a 5 to 50 kg melt, 15 to 25 mm is common. Larger melts use thicker walls to resist charging impact.
Related Graphite Products
Hot Tags: graphite crucible liner for induction melting - inner liner for metal melting, China graphite crucible liner for induction melting - inner liner for metal melting manufacturers, suppliers, factory, 3 kg graphite crucible, clay crucible, crucible chemistry lab, graphite carbon crucible, graphite crucible for electronics, graphite foundry crucibles
