Graphite Solder Pot For Wire Tinning Lines

A solder pot sits at 250 to 320 C all shift, and the flux that floats on the surface attacks most crucible materials. Graphite resists the flux and does not react with tin, so the bath stays clean and the wire comes out with an even coating.
The pot is machined as a thick-walled cylinder with a lip that guides the wire and a spout for dross removal. Wall thickness is set by the pot diameter so the rim does not sag when the bath is emptied and refilled.
Key Features
-
Flux-resistant wall - graphite does not react with rosin or halide flux at tinning temperature
-
Even wall temperature - high thermal conductivity limits cold spots that cause dewetting
-
Guided wire lip - the rim profile steers the wire through the bath without touching the wall
-
Dross spout - a machined spout lets the operator skim dross without disturbing the bath
-
Thick base - the base carries the bath weight without bowing on the heater plate
-
Capacity options - pot volume matched to the tinning line throughput
Technical Specifications
| Property | Typical Value |
| Grade | fine-grain, resin-free |
| Density | 1.85 - 1.92 g/cm3 |
| Ash content | below 0.05 percent |
| Inner diameter | 60 - 300 mm |
| Depth | 60 - 250 mm |
| Wall thickness | 10 - 30 mm |
| Base thickness | 15 - 35 mm |
| Lip radius | 3 - 10 mm |
| Operating temperature | 250 - 350 C |
| Thermal conductivity | 110 - 145 W/m.K |
| Porosity | sealed surface, open porosity below 5 percent |
| Supply form | pot with lid or pot alone |
Applications & How to Use
Wire tinning machines
the pot holds the solder bath the wire passes through
Component lead timing
a shallow pot fits benchtop tinning stations
Stranded cable ends
guided lip keeps the strands together as they leave the bath
Solder bath replacement
the pot is a drop-in replacement for a cracked metal pot
Small batch assembly
a compact pot suits low-volume hand tinning
Why Choose Jincheng
- Pots are machined from a single billet, so there is no seam for flux to attack
- Wall thickness is set from the diameter to keep the rim true after emptying
- The base is thick enough to sit flat on a heater plate without a heat spreader
- Sealed surface limits solder penetration into open porosity
- Spouts and lips are cut to the machine drawing, not to a catalogue shape
- Pots are pressure checked for wall soundness before shipment
FAQ
Will the solder wet the graphite
No. Solder does not wet graphite, which is why the pot stays clean and dross is easy to skim
Can the pot be used with lead-free solder
Yes, and graphite handles the higher temperature of lead-free baths better than most metal pots
How is the pot heated
Usually from a flat heater plate under the base, so the base thickness is set for even conduction
Does flux attack graphite
Rosin and halide fluxes do not attack graphite at tinning temperature, unlike iron or ceramic pots
Related Graphite Products
Graphite Crucible For Aluminium Melting
Hot Tags: graphite solder pot for wire tinning lines, China graphite solder pot for wire tinning lines manufacturers, suppliers, factory, 1 kg graphite crucible, casting clay graphite, clay and graphite, glass crucible chemistry, graphite double ring crucible, high density graphite crucibles