Graphite Mold Liner For Copper Ingot Casting %MAINIMG% A graphite mold liner is the inner shell of an ingot mold: the part that actually touches the solidifying copper, while a steel or cast-iron backing plate carries the mechanical load. Lining an ingot mold with graphite gives a smooth,...
Category
Graphite Mold
Share to
Description

Graphite Mold Liner For Copper Ingot Casting

Graphite Mold Liner For Copper Ingot Casting

A graphite mold liner is the inner shell of an ingot mold: the part that actually touches the solidifying copper, while a steel or cast-iron backing plate carries the mechanical load. Lining an ingot mold with graphite gives a smooth, non-wetting surface, so the ingot shrinks away cleanly and the surface finish is good enough that the ingot needs less scalping.

Jincheng supplies liners as matched sets for rectangular, round and hexagonal ingot sections, with the wall thickness chosen so the liner survives the thermal gradient between the melt and the water-cooled jacket. Liners are machined with a taper that matches the mold, and each set is marked so the four sides of a rectangular mold are assembled in the same order.

Key Features

  • Non-wetting casting surface - Molten copper does not wet graphite, so the ingot shell pulls away as it shrinks and the surface comes out smooth instead of torn.

  • Replaceable without scrapping the mold - When the liner wears, the backing plate stays in service and only the liner is replaced, which cuts mold maintenance cost.

  • Taper matched to the mold - The liner is machined with the same taper as the mold body, so it seats against the backing plate without a gap that would trap metal.

  • Wall thickness for the thermal gradient - Thicker walls near the hot end and thinner walls at the base keep the liner from cracking while holding enough insulation.

  • Set identity marking - Rectangular molds have four liners; each is stamped with its position so a set can be reassembled in the original orientation.

  • Machined joint faces - Corners are machined so the liners meet with a controlled gap, which limits metal penetration between the plates.

Technical Specifications

Property Typical Value
Material Fine-grain moulded graphite
Bulk density 1.75 to 1.88 g/cm3
Flexural strength 45 to 85 MPa
Ash content Below 0.2 percent
Ingot section Rectangular, round or hexagonal
Liner length 300 to 2000 mm
Wall thickness 10 to 40 mm
Taper 0.5 to 2 degrees per side
Thickness tolerance +/-0.5 mm
Joint gap between liners 0.5 mm maximum
Surface finish Ra 1.6 to 3.2 um on the casting face
Service temperature Up to 1200 C in inert gas or reducing atmosphere

Applications & How to Use

Copper wire rod ingot casting

Liners are fitted into water-cooled molds; the smooth graphite face reduces the scalping depth on the ingot surface.

Oxygen-free copper slab casting

Rectangular liner sets are used where surface cleanliness matters for subsequent rolling.

Brass and bronze billet casting

Liners handle the higher zinc vapour load because the graphite surface resists penetration better than bare steel.

Precious metal ingot molds

Small round liners give a clean ingot surface that reduces metal loss during finishing.

Mold refurbishment

A worn steel mold is rebuilt by machining the backing plate and fitting new graphite liners, which restores the original section.

Why Choose Jincheng

  • Liners are supplied as identified sets, so a four-sided mold is assembled correctly after a reline.
  • We machine the taper from the mold drawing rather than from a sample, which keeps the liner and the backing plate in contact.
  • Wall thickness can be varied along the length where the thermal gradient is steepest.
  • The casting face is machined fine enough that the ingot surface does not need heavy conditioning.
  • Replacement liners are quoted against the original set number, so a repeat order cannot drift.
  • Long liners are shipped in cradles with the tapered faces protected.

FAQ

Why line an ingot mold with graphite instead of using bare steel?

Graphite is non-wetting and does not heat check, so the ingot surface is smoother and the mold lasts longer between repairs.

Can one liner be replaced instead of the whole set?

Yes, but the new liner should be machined to the same taper as the remaining ones; we keep the set record so a single replacement still matches.

What joint gap is acceptable between liners?

We machine to 0.5 mm maximum. A wider gap lets molten copper penetrate and makes the ingot hard to strip.

How long does a liner last?

Life depends on metal temperature and tonnage. In copper rod casting customers typically reline every 6 to 18 months.

Do you machine round liners for vertical casting?

Yes, round liners from 100 to 400 mm bore are machined with the taper and the bottom seat included.

Related Graphite Products

Graphite Ingot Mold For Copper And Gold

Graphite Die Insert For Brass Gravity Casting

Hot Tags: graphite mold liner for copper ingot casting - replaceable cavity liner, China graphite mold liner for copper ingot casting - replaceable cavity liner manufacturers, suppliers, factory, 1kg ingot mould, graphite ingot mold, graphite mold, graphite molds for jewelry, hydrogen fuel cell plates, smelting graphite molds

Send Inquiry