Refurbishing Graphite Parts: What Can Be Saved And What Cannot

Some Wear Is Recoverable
Surface wear, glaze loss and light erosion on a functional face can often be recovered by re-machining or re-coating, provided there is enough material left to remove the worn layer and still meet the drawing.
Refurbishment is usually economic for large parts where the material cost dominates, and rarely economic for small consumables where the machining cost is most of the price.
What Cannot Be Recovered
Cracks are the hard limit. A cracked part cannot be welded or brazed back to structural integrity, because graphite does not accommodate the thermal stress of a repair. Cracks that reach a sealing face condemn the part.
Deep oxidation is the second limit: a hot face that has lost several millimetres has also lost strength, and re-machining exposes a new surface with different properties from the original.
Deciding Whether To Refurbish
Measure the remaining section at the worn area and compare with the minimum in the drawing. Check for cracks with dye penetrant before committing to machining, since a crack found after machining wastes both efforts.
Record the original machining date and service hours, so that the decision to refurbish or replace is made on evidence rather than on the part's appearance.
Conclusion
Refurbish where the section allows and no crack exists; replace where either condition fails. Penetrant check first, measure the section second, then decide.