Tolerances On Graphite Drawings: Where Machinists Waste Money

Graphite Is Not Steel
A drawing copied from a steel part often carries tolerances that graphite cannot hold cheaply and does not need. Graphite is machined easily but is brittle and slightly porous, so a tolerance that depends on a rigid, homogeneous material behaves differently here.
The cost drivers are flatness, parallelism and surface finish on large faces, not the nominal dimensions. A 0.02 mm flatness call-out on a 300 mm plate can double the machining time.
Which Tolerances Matter
Specify flatness and parallelism where they affect function: a sealing face, a wafer contact face or a brazing pocket floor. Specify surface finish only on the faces that see contact or release, and leave the rest at a general value.
Dimensional tolerances on features that are located by an assembly fixture can often be relaxed, because the fixture sets position and the part only has to fit.
Inspection And Records
Ask for the inspection values on the functional faces and for the measurement method, since a flatness figure taken on a surface plate without the service support can mislead. Keep the batch record with the part number so a replacement can be compared.
Where a part is a consumable, agree a wear allowance on the functional dimension rather than a tolerance stack that no used part can meet.
Conclusion
Put tight tolerances where the part functions and relax the rest. State the measurement method, and agree wear allowances on consumables. Drawings are reviewed before machining on request.
Machined graphite parts and material grades are listed on the product index; for grade comparison see the selection checklist.